Planning operations

France

Test brief report (Building located in Paris suburb)

The building was a difficult one because the flock was coated with a paint layer added in the early nineties.

An area of 30 m2 of flock was treated by spraying with 10-12 liters of ATP Sol 50/50 diluted with water, or about 300 g ATP Sol per m2.

The spraying went well.

Despite the presence of the paint layer, the product has entered entirely. The product is foaming. It forms a white froth. We remarked a good distribution over the treated areas. This scum disappears drying.

The scrapings flock operations were undertaken after 12 hours of drying.

We reduced the additive rate in the formula with the aim to engluage dust and to consolidate mechanical flock in a way to its abduction. This reduction additive reduces the formulation cost.
 
Europe

Tests are presently pursued in Spain & Netherlands.

© 2009 IR & Amiante